Manufacturer's welding procedure specification (WPS) POLBAN Location: WTC-ATB POLBAN, Bandung, Indonesia Examiner or Test Body: Ir. Sutrimo, M.Eng Manufacturer's Procedure No.: WPS-WTC 003.5 Method of Preparation and Cleaning: Grinding Reference No. : WPS-WTC 04.3 Parent Material Specificati...
Manufacturer's welding procedure specification (WPS) POLBAN Location: WTC-ATB POLBAN, Bandung, Indonesia Examiner or Test Body: Ir. Sutrimo, M.Eng Manufacturer's Procedure No.: WPS-WTC 003.5 Method of Preparation and Cleaning: Grinding Reference No. : WPS-WTC 04.3 Parent Material Specification: St 37 (S 235 JR) Manufacturer : POLBAN Welder's Name : Idham K, ST., MT Material Thickness (mm) : 8 Welding Process : 111 (SMAW) Outside Diameter (mm) : - Type: Plate - BW (V - Joint) Welding Position : PA (1G) Weld Preparation Details (Sketch): *) Joint Design Welding Sequence/Layer Welding Details Run Process Size of Filler Material mm Current A Voltage V Type of Current/ Polarity Wire Feed Speed m/min Travel Speed *) cm/min Heat Input *) KJ/cm 1 111 2.6 60 - 70 19 DC EP - 8 - 10 - 2 111 3.2 70 - 80 19 ~ - DC EP - 6 - 8 .._ - Filler Metal Other Information') Classification & Trade Name: e.g. Weaving: Maximum of Run in mm: AWS E 7016 2.6 mm & 3.2 mm Oscillation: Amplitude, Frequency, Dwell Time: Any Special Baking and Drying: Pull Welding Details : - Gas/Flux: Stand Off Distance : - - Shielded : - Plasma Welding Details: - - Backing : - Torch Angle: 70o Gas Flow Rates: - Shielded : - - Backing : - Tungsten Electrode Type/Size: Details of Back Gouging/Backing: Preheat Temperature : - Inter pass Temperature : - *) ... if applicable Post Weld Heat Treatment and/or Aging: n.a. ... not applicable Time - Temperature – Method Welder Stamp: W.01.001 Heating and Cooling Rates:*) Manufacturer Examiner or Test Body Name, Date, Signature Name, Date, Signature 8 mm 2 – 3 mm 1.5 – 2 mm 60°...